GA-9035A/B ƒe agbalẽa
Herchy .
| Nusiwo li: | |
|---|---|
| Agbɔsɔsɔ: | |
Dodokpɔ: 1% le atike si daa gbe le ame ŋu (50% ƒe atike si wotsɔ DBPMH wɔe le silicon-gum me), 175° x 5min x 15MPa.
| Adzɔnuwo ƒe nɔnɔmetatawo . | ||||||
| Nu si wowɔ | GA-9035A/B ƒe agbalẽa |
GA-9041A/B ƒe agbalẽa | GA-9051A/B ƒe agbalẽa | GA-9061A/B ƒe agbalẽa | GA-9071A/B ƒe agbalẽa | GA-9081A/B ƒe agbalẽa |
| Dzedzeme | Si me kɔ | |||||
| WilliamPlasticity . |
150 |
190 |
210 |
240 |
270 |
290 |
| Sesẽ (Shorea) . |
36 |
40 |
50 |
60 |
70 |
80 |
| Density(G/CM3) . | 1.10 |
1.13 |
1.16 |
1.18 |
1.19 |
1.21 |
| Tensile ƒe ŋusẽ (MPA) . |
10 |
9.0 |
10.0 |
10.0 |
9.5 |
9.0 |
| Elongation(%) . | 1050 |
900 |
700 |
600 |
500 |
400 |
| Aɖatsiŋusẽ (kn/m) . | 25 |
30 |
35 |
35 |
35 |
35 |
| Gbugbɔgadzɔ(%) . |
60 |
55 |
55 |
50 |
50 |
|