Tel: +86 15221953351 E-mail: info@herchyrubber.com
Please Choose Your Language
Ngwaahịa
Ị nọ ebe a: Ụlọ » Ngwaahịa » Rubber Synthesis » Silikoni VMQ GA -9035A/B Platinum catalyzed silicone roba maka ahụike (HCR)

nbudata

Kekọrịta na:
bọtịnụ nkekọrịta Facebook
bọtịnụ ikesa twitter
bọtịnụ nkekọrịta akara
bọtịnụ nkekọrịta wechat
bọtịnụ njikọ njikọ
bọtịnụ nkekọrịta pinterest
bọtịnụ ịkekọrịta WhatsApp
kekọrịta bọtịnụ nkekọrịta a

GA-9035A/B Platinum catalyzed silicone roba maka ahụike (HCR)

Ngwa: dabara adaba maka imepụta ngwaahịa ọgwụ.
Isi njirimara: ike dị elu, nghọta dị elu, ihe onwunwe na-adịghị mma na-acha odo odo, na-adịghị egbu egbu na enweghị ụtọ, gafere nkwenye nke RoHS, REACH, FDA, LFGB.Gafee ule nke 1S010993 biocompatibility.
  • GA-9035A/B

  • Herchy

Nnweta:
Ọnụọgụ:

Nnwale: 1% nke onye na-agwọ ọrịa (50% tapawa nke DBPMH na silicone gum), 175° x 5min x 15MPa.


Ngwa ngwaahịa
Ngwaahịa GA-9035A/B
GA-9041A/B GA-9051A/B GA-9061A/B GA-9071A/B GA-9081A/B
Ọdịdị N'ụzọ doro anya
Williamplasticity
150
190
210
240
270
290
Isi ike (ShoreA)
36
40
50
60
70
80
Njupụta (g/cm3) 1.10
1.13
1.16
1.18
1.19
1.21
Ike tensile (MPa)

10
9.0
10.0
10.0
9.5
9.0
Mgbatị(%) 1050
900
700
600
500
400
Ike akwa mmiri (kN/m) 25
30
35
35
35
35
Nlaghachi(%)
60
55
55
50
50








Nke gara aga: 
Osote: 

Njikọ ngwa ngwa

Ngwaahịa anyị

OZI MKPỌTỤRỤ

Tinye: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Nwebiisinka     2023 Shanghai Herchy Rubber Co., Ltd. map saịtị |   Amụma nzuzo | Nkwado Site Leadong.