GA-9035A/B Platinum katalised silikon rɔba fɔ mɛdikal (HCR)

Aplikeshɔn: fayn fɔ prodyuz mɛrɛsin prɔdak.
Ki ficha dɛm: ay trɛnk, ay transperɛns, gud anti-yɔlɔ prɔpati,nɔ-tɔxik ɛn teistlɛs, pas di ɔthɛntishɔn fɔ RoHS, REACH, FDA, LFGB.Pas di tɛst fɔ 1S010993 biocompatib山ty.
  • GA-9035A/B we de na di wɔl

  • Herchy bin de du am

Di tin dɛn we yu kin gɛt:
Kwantiti: .

Tεst: 1% pan di kכring ejen (50% paste fכ DBPMH insay silikon gכm), 175° x 5min x 15MPa.


Prodakt paramita dɛn
Sɔntin GA-9035A/B we de na di wɔl
GA-9041A/B we de na di wɔl GA-9051A/B we de na di wɔl GA-9061A/B we de na di wɔl GA-9071A/B we de na di wɔl GA-9081A/B we de na di wɔl
Aw a luk Klia
Wiliamplastisiti
150
190
210
240
270
290
Di hadnɛs (ShoreA) .
36
40
50
60
70
80
Densiti(g/cm3) . 1.10
1.13
1.16
1.18
1.19
1.21
Tensile strɛngth (MPa) .

10
9.0
10.0
10.0
9.5
9.0
Elongation(%) we de go bifo. 1050
900
700
600
500
400
Tear strɛngth (kN/m) . 25
30
35
35
35
35
Ribaund(%) .
60
55
55
50
50








Bifo: 
Nɛks: 

KWƐK LINK DƐN

WI PRODƆKT DƐN

INFƆMƐSHƆN FƆ KƆNTƐKT

Ad: No.33, Len 159, Taiye Rod, Fengxian Distrikt, Shanghai
Tɛl / WatsAp / Skype: +86 15221953351
Kopirayt     2023 Shanghai Herchy Rɔba Kɔmni, Ltd. Sitemap fɔ di sayt |   Prayvesi Polisi | Sɔpɔt Bay Leadong we de na di wɔl.