GA-9035A/B Platinum catalyzed silicone rubber no ka lapaau (HCR)

Noi: kūpono no ka hana ʻana i nā huahana lapaʻau.
ʻO nā hiʻohiʻona nui: ka ikaika kiʻekiʻe, ke aniani kiʻekiʻe, ka waiwai anti-yellowing maikaʻi, ʻaʻohe mea ʻawaʻawa a me ka ʻono ʻole, hele i ka hōʻoia o RoHS, REACH, FDA, LFGB.Pass i ka hōʻike o 1S010993 biocompatib山ty.
  • GA-9035A/B

  • Herchy

Loaʻa:
Nui:

Ho'āʻo: 1% o ka lāʻau lapaʻau (50% paʻi o DBPMH i loko o ka silicone gum), 175° x 5min x 15MPa.


Nā palena huahana
Huahana GA-9035A/B
GA-9041A/B GA-9051A/B GA-9061A/B GA-9071A/B GA-9081A/B
Ka nana aku Alohilohi
Williamplasticity
150
190
210
240
270
290
Paʻakikī (ShoreA)
36
40
50
60
70
80
Māmā (g/cm3) 1.10
1.13
1.16
1.18
1.19
1.21
Ka ikaika uʻi (MPa)

10
9.0
10.0
10.0
9.5
9.0
Elongation(%) 1050
900
700
600
500
400
Kaha waimaka (kN/m) 25
30
35
35
35
35
Hoʻihoʻi hou (%)
60
55
55
50
50








Mua: 
Aʻe: 

NUI WIWIKI

KO MAKOU HANA

IKE HOPE

Hoʻohui: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Kuleana kope     2023 Shanghai Herchy Rubber Co., Ltd. Palapala kahua |   Kulekele pilikino | Kākoʻo Na Leadong.