Test: 1% of curing agent (50% paste of DBPMH in silicone gum), 175° x 5min x 15MPa
| Product parameters | ||||||
| Product | GA-7005 | GA-7010 | GA-3005 | GA-3010 | GA-1093W | GA-3091 |
| Appearance | Translucent | |||||
| Williamplasticity | 50 | 80 | 50 | 80 | 340 | 380 |
| Hardness (ShoreA) | 5 | 10 | 5 | 10 | 90 | 90 |
| Density(g/cm3) | 1.05 | 1.08 | 1.05 | 1.07 | 1.23 | 1.25 |
| Tensilestrength (MPa) | 1.5 | 2.5 | 1.5 | 3 | 5 | 7 |
| Elongation(%) | 850 | 850 | 850 | 900 | 40 | 80 |
| Tearstrength (kN/m) | 4 | 6 | 5 | 8 | 12 | 20 |