GA- 7005
Earcach
| Infhaighteacht: | |
|---|---|
| Cainníocht: | |
Tástáil: 1% den ghníomhaire leigheas (50% de DBPMH a ghreamú i guma silicone), 175° x 5min x 15MPa
| Paraiméadair táirge | ||||||
| Táirge | GA- 7005 |
GA-7010 | GA- 3005 | GA-3010 | GA-1093W | GA- 3091 |
| Dealramh | Tréshoilseach | |||||
| Williamplasticity |
50 |
80 |
50 |
80 |
340 |
380 |
| Cruas (ShoreA) |
5 |
10 |
5 |
10 |
90 |
90 |
| Dlús(g/cm3) | 1.05 |
1.08 |
1.05 |
1.07 |
1.23 |
1.25 |
| Neart teanntachta (MPa) |
1.5 |
2.5 |
1.5 |
3 |
5 |
7 |
| Fadú(%) | 850 |
850 |
850 |
900 |
40 |
80 |
| neart cuimilt (kN/m) | 4 |
6 |
5 |
8 |
12 |
20 |