GA-7005
Herchy
| Avanoa: | |
|---|---|
| Aofa'i: | |
Su'ega: 1% o le vaila'au fa'amalolo (50% fa'apipi'i o le DBPMH i le pulu silicone), 175° x 5min x 15MPa
| Fa'atauga o oloa | ||||||
| Oloa | GA-7005 |
GA-7010 | GA-3005 | GA-3010 | GA-1093W | GA-3091 |
| Fa'aaliga | Translucent | |||||
| Williamplasticity |
50 |
80 |
50 |
80 |
340 |
380 |
| Malosi (ShoreA) |
5 |
10 |
5 |
10 |
90 |
90 |
| Malosi (g/cm3) | 1.05 |
1.08 |
1.05 |
1.07 |
1.23 |
1.25 |
| Malosi (MPa) |
1.5 |
2.5 |
1.5 |
3 |
5 |
7 |
| Fa'atele(%) | 850 |
850 |
850 |
900 |
40 |
80 |
| Malosi loimata (kN/m) | 4 |
6 |
5 |
8 |
12 |
20 |