GA-7005 Silicone Rubber Yepamusoro Kana Yakaderera Kuoma (HCR)

Chishandiso: chakakodzera kugadzira zvigadzirwa zvine zvinodiwa zve-ultra-high kana -lowhardness, senge, kuputira kwepurasitiki, kusatsvedza pad, pad yeshangu, pedhi yetsoka, kitchenware, zvisimbiso, uye zvakasiyana-siyana nezvimwe.   
Akakosha maficha: Ultra-yakakwirira kana -yakadzika kuomarara, kupfava kwakanaka, pfuura huchokwadi hweRoHS, REACH, uye FDA
  • GA-7005

  • Herchy

Kuwanikwa:
Huwandu:

Muedzo: 1% yekurapa mumiririri (50% paste yeDBPMH mune silicone gum), 175 ° x 5min x 15MPa

Product parameters
Product GA-7005
GA-7010 GA-3005 GA-3010 GA-1093W GA-3091
Chitarisiko Translucent
Williamplasticity
50
80
50
80
340
380
Kuoma (ShoreA)
5
10
5
10
90
90
Density(g/cm3) 1.05
1.08
1.05
1.07
1.23
1.25
Tensilestrength (MPa)

1.5
2.5
1.5
3
5
7
Elongation(%) 850
850
850
900
40
80
Kusimba kwemisodzi (kN/m) 4
6
5
8
12
20





Zvakapfuura: 
Zvinotevera: 

KUKURUMIDZA ZVINONYANYA

ZVINHU ZEDU

CONTACT INFORMATION

Wedzera: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |   Privacy Policy | Support By Leadong.