GA-7005
Herchy
| Argaeledd: | |
|---|---|
| Nifer: | |
Prawf: 1% o asiant halltu (50% past o DBPMH mewn gwm silicon), 175 ° x 5 munud x 15MPa
| Paramedrau cynnyrch | ||||||
| Cynnyrch | GA-7005 |
GA-7010 | GA-3005 | GA-3010 | GA- 1093W | GA- 3091 |
| Ymddangosiad | Tryleu | |||||
| Williamplastigedd |
50 |
80 |
50 |
80 |
340 |
380 |
| Caledwch (ShoreA) |
5 |
10 |
5 |
10 |
90 |
90 |
| Dwysedd(g/cm3) | 1.05 |
1.08 |
1.05 |
1.07 |
1.23 |
1.25 |
| Cryfder tynnol (MPa) |
1.5 |
2.5 |
1.5 |
3 |
5 |
7 |
| elongation(%) | 850 |
850 |
850 |
900 |
40 |
80 |
| Cryfder dagrau (kN/m) | 4 |
6 |
5 |
8 |
12 |
20 |