GA-7005 Rapa Hikaona o te Maamaa Teitei, Hakaiti ranei (HCR)

Te tono: e tika ana mo te whakaputa hua me nga whakaritenga o te ultra-high or -lowhardness, penei i te, takai kirihou, papa kore-paheke, papa hu, papa waewae, taputapu kihini, hiri, me etahi atu mea.   
Ko nga ahuatanga matua: te tino teitei, te -iti ranei te pakeke, te ngawari, te whakamanatanga o RoHS, REACH, me te FDA
  • GA-7005

  • Herchy

Watea:
Rahi:

Whakamatau: 1% o te kaihoko whakaora (50% te whakapiri o te DBPMH i roto i te kapia silicone), 175° x 5min x 15MPa

Tawhā hua
Hua GA-7005
GA-7010 GA-3005 GA-3010 GA-1093W GA-3091
Te ahua Puatarangi
Williamplasticity
50
80
50
80
340
380
Maama (ShoreA)
5
10
5
10
90
90
Kiato(g/cm3) 1.05
1.08
1.05
1.07
1.23
1.25
Te kaha (MPa)

1.5
2.5
1.5
3
5
7
Whakaroa(%) 850
850
850
900
40
80
Te Roimata (kN/m) 4
6
5
8
12
20





Tōmua: 
Panuku: 

NGA LINKO Tere

O TATOU HUA

HE KORERO WHAKAPAKI

Tāpirihia: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Waea / WhatsApp / Skype: +86 15221953351
Ī-mēra:  info@herchyrubber.com
Mana pupuri     2023 Shanghai Herchy Rubber Co., Ltd. Mahere pae |   Kaupapahere Tūmataiti | Tautoko Na Leadong.