GA-7005
Herchy
| Kasedhiyan FDA: | |
|---|---|
| Jumlah: | |
Tes: 1% agen pengawet (50% tempel DBPMH ing permen karet silikon), 175° x 5min x 15MPa
| Parameter produk | ||||||
| produk | GA-7005 |
GA-7010 | GA-3005 | GA-3010 | GA-1093W | GA-3091 |
| Penampilan | Tembus | |||||
| Williamplastisitas |
50 |
80 |
50 |
80 |
340 |
380 |
| Kekerasan (ShoreA) |
5 |
10 |
5 |
10 |
90 |
90 |
| Kapadhetan (g/cm3) | 1.05 |
1.08 |
1.05 |
1.07 |
1.23 |
1.25 |
| Daya Tarik (MPa) |
1.5 |
2.5 |
1.5 |
3 |
5 |
7 |
| Elongasi (%) | 850 |
850 |
850 |
900 |
40 |
80 |
| Kekuwatan sobek (kN/m) | 4 |
6 |
5 |
8 |
12 |
20 |