Deuchainn: 1% de àidseant leigheas (50% paste de DBPMH ann an guma silicone), 175 ° x 5min x 15MPa
| Paramadairean toraidh | ||||||
| Bathar | GA-7005 |
GA-7010 | GA-3005 | GA-3010 | GA-1093W | GA-3091 |
| Coltas | Tar-shoilleir | |||||
| Williamplasticity |
50 |
80 |
50 |
80 |
340 |
380 |
| cruas (CladachA) |
5 |
10 |
5 |
10 |
90 |
90 |
| Dlùths (g/cm3) | 1.05 |
1.08 |
1.05 |
1.07 |
1.23 |
1.25 |
| Neart tensile (MPa) |
1.5 |
2.5 |
1.5 |
3 |
5 |
7 |
| Leudachadh (%) | 850 |
850 |
850 |
900 |
40 |
80 |
| Neart deòir (kN/m) | 4 |
6 |
5 |
8 |
12 |
20 |