Isku-darka caagga, tijaabooyin badan oo isku-duubni ah ayaa la sameeyaa marka loo eego tijaabooyinka qallafsanaanta joogtada ah. Sida hoos looga wada hadli doono, dhinacyo badan oo ka mid ah barxadda caagga ah waxay saameeyaan sifooyinka qallafsanaantooda. Waa in halkan lagu xuso in qallafsanaanta joogtada ah iyo qallooca joogtada ahi ay yihiin laba sifo oo kala duwan. Sidaa darteed, waxa hagaajiya isku-buufinta is-beddelka joogtada ah maahan inay hagaajiso qallafsanaanta joogtada ah, iyo lidka ku ah. Intaa waxaa dheer, alaabooyinka xirmooyinka caagga ah, qallafsanaanta joogtada ah ee ciriiriga ah maaha saadaal wanaagsan ee cadaadiska xiridda ama waxqabadka xiridda. Caadi ahaan, way sii adkaanaysaa tijaabada nasinta cadaadiska cadaadisku waa in la sameeyaa, si fiican ayaa loo saadaaliyaa waxqabadka xidhitaanka alaabta.
Nidaamyada tijaabada ah ee soo socda ayaa loo isticmaalaa si loo hagaajiyo waxqabadka cilladda joogtada ah ee caagga. Xusuusin: Hab-maamuusyadan tijaabada ah waxaa laga yaabaa inaan lagu dabaqi karin dhammaan kiisaska. Intaa waxaa dheer, doorsoome kasta oo yarayn kara qallafsanaanta joogtada ah ee isku-buuqa ama xiisadda waxay saameyn kartaa guryaha kale mana lagu soo hadal qaadi doono qoraalka.
1. nidaamka vulcanization
Tixgeli isticmaalka peroxides sida walxaha vulcanizing, kaas oo samayn kara CC bonds-isku-xidhan oo markaa wanaajinaya qallafsanaanta joogtada ah ee caagga. Vulcanization ee caagga ethylene propylene ee leh peroxide waxay yarayn kartaa isku-duubnaanta cilladda joogtada ah ee caagga. Faa'iidooyinka ay peroxide ku leedahay baaruuddu waa fudaydka maaraynta peroxide iyo khalqiga joogtada ah ee hooseeya ee caagga.
2. Waqtiga Vulcanization iyo heerkulka
Heerkulka vulcanization sare iyo wakhtiga vulcanization oo dheer waxay kordhin kartaa heerka vulcanization sidaas darteed waxay yaraynaysaa isku xidhka caagga.
3. Cufnaanta isku xirta
Kordhinta cufnaanta isgoysyada ee caaggu waxay si wax ku ool ah u yareeyn kartaa isku-duubnaanta cilladda joogtada ah ee caagga.
4. Nidaamka vulcanization sulfur
Si loo yareeyo qallafsanaanta joogtada ah ee xarunta EPDM oo loo hagaajiyo caabbinta kulaylka, waxaan tixgelin karnaa nidaamkan 'qalafsanaanta hooseeya' nidaamka vulcanization (mass): baaruud 0.5PHR, ZDBC 3PHR, ZMDC 3PHR, DTDM 2PHR, TMTD3PHR.
Nooca W neoprene, isticmaalka dardar-geliyaha diphenylthiourea wuxuu ka dhigi karaa caag leh cillad hoose oo qallafsan, laakiin iska ilaali isticmaalka CTP sida wakiilka kookaha, inkasta oo ay sii dheerayn karto wakhtiga kuleylka, laakiin waxay leedahay dhaawac dheeraad ah oo ku yimaada cilladda cilladda joogtada ah.
Wixii caag NBR ah, in nidaamka vulcanization la doortay, xaddiga baaruud waa in la dhimo, isku day in aad isticmaasho baaruud si ay u bixiyaan jirka sida TMTD ama DTDM si ay u beddelaan qayb ka mid ah baaruud ah, xubno baaruud yar yar hagaajin doonaa riixo waxqabadka qallafsan joogto ah ee caag ah. Nidaamka vulcanization ee leh HVA-2 iyo hyposulfuramide waxay ka dhigi karaan caag leh cillad hoose oo cillad joogto ah.
5. nidaamka vulcanization peroxide
Doorashada BBPIB peroxide waxay ku siin doontaa caagga isbeddel joogto ah oo wanaagsan oo cadaadis ah. Nidaamyada vulcanization peroxide, isticmaalka co-crosslinkers waxay kordhisaa unsaturation ee nidaamka, taas oo iyaduna keenta cufnaanta crosslink sare, maxaa yeelay, crosslinking ee xagjirka lacag la'aan ah oo curaarta unnsaturated waxay u dhacdaa si ka sahlan marka loo eego qaadashada hydrogen ee silsiladaha saturated. Isticmaalka isku-tallaabta-isku-tallaabta waxay beddelaan nooca isku-xidhka isku-xidhka waxayna sidaas wanaajisaa isku-buuqa sifooyinka cilladda joogtada ah ee koollada.
6. vulcanization ka dib
Waxaa jira vulcanization by-products inta lagu guda jiro habka vulcanization, iyo habka-vulcanization post-vulcanization atmospheric cadaadiska atmospheric u ogolaanaya kuwan by-products in la sii daayo, siinaya cinjirka set cadaadis hoose.
7. Fluoroelastomer FKM/Bisphenol AF Vulcanization
Fluoroelastomers, isticmaalka wakiilka vulcanizing bisphenol halkii laga isticmaali lahaa wakiilka vulcanizing peroxide waxay siin kartaa caagga hoos u dhac joogto ah oo ku yimaada cadaadis.
8. Saamaynta miisaanka unugyada
Qaabka caagga ah, doorashada caagga leh celceliska culeyska kelliga ah ee weyn ayaa si wax ku ool ah u yareeyn kara ciribtirka cilladda joogtada ah ee caagga.
Caag NBR ah, caagga leh mawqifka Mooney ee sarreeya waa in la isticmaalaa, kaas oo ka dhigi kara caag yar oo cidhiidhi ah cillad joogto ah.
9. Neoprene
Nooca W neoprene wuxuu leeyahay cillad joogto ah oo cadaadis hoose ah marka loo eego nooca G neoprene.
10. EPDM
Si aad u samayso caag leh cidhiidhi hoose oo qallafsan, isku day inaad iska ilaaliso isticmaalka caag EPDM leh crystallinity sare.
11. NBR
NBR, kaas oo ah emulsion polymerized leh calcium chloride sida xinjirowga dhiigga, sida caadiga ah waxay leedahay go'an cadaadis hoose.
Wixii caag NBR ah, haddii aad rabto in aad diirada saarto ay riixo waxqabadka qallafsanaan joogto ah, ka dibna isku day in aad doorato noocyo leh laamo sare iyo silsilad sare isku xidha ama noocyo leh content acrylonitrile hoose.
12. Ethylene-acrylate caag ah
Caagadaha AEM, wakiilada vulcanizing peroxide waxay ku siin karaan cadaadis hoose marka loo eego wakiilada vulcanizing diamine.
13. homogenizers-ku-saleysan-resin
Ka fogow isticmaalka homogenizers-ku-salaysan resin-ka ee xeryahooda caagga ah, maadaama ay tani kordhinayso isku-xidhka xarunta.
14. Buuxiyeyaasha
Yaraynta buuxinta, qaab-dhismeedka iyo aagga gaarka ah ee buuxinta (kordhinta cabbirka qaybta) waxay sida caadiga ah yaraynaysaa isku-buufinta. Isla mar ahaantaana, kordhinta dhaqdhaqaaqa dusha sare ee buuxintu waxay sidoo kale wanaajin kartaa iska caabbinta isku-dhafka ee xarunta.
15. Silica
Buuxiyaha silica hoose ee xarunta ayaa yarayn doona isku-buufinta. Si loo helo cadaadis hooseeya, waxaa lagama maarmaan ah in laga fogaado buuxinta sare ee silica. Haddii tirada buuxintu ay ka sarreyso 25 qaybood (mass), qallafsanaanta joogtada ah ee xaruntu waxay noqotaa mid weyn.
16. Wakiilka isku xirka Silane
Iyadoo la tixgalinayo isticmaalka wakiilka isku-xidhka silane ee tirada sare ee buuxinta silica degdega ah, isku-buufinta cilladda joogtada ah ee koollada waa la yarayn karaa. Wakiilka isku xidhka Silane waxa uu yarayn karaa cidhiidhiga qallafsanaanta joogtada ah ee caag silica ka buuxsantay, waxa kale oo uu yarayn karaa cidhiidhiga qallafsanaanta joogtada ah ee buuxinta nooca silicate sida dhoobada, budada talcum iyo caag kale oo la buuxiyey.
17. caagadaha
Yaraynta cadadka buuxinta caagga caagga ah ee ku jira caagga waxay caadi ahaan hoos u dhigi doontaa isku-buufinta cilladda joogtada ah ee caagga.