GA-2230
Herchy
| Kuboneka: | |
|---|---|
| Umubare: | |
Ikizamini: Ikigereranyo cya A / B cya 1: 1, 130 ° C x 5min x 15MPa.
| Ibipimo byibicuruzwa | ||||||
| Ibicuruzwa | GA-2230 | GA-2240 | GA-2250 | GA-2260 | GA-2270 | |
| Kugaragara | Mucyo | |||||
| Viscosity (Pa.s) |
10 | 10 | 8 | 5 | 5 | |
| Gukomera (ShoreA) | 30 | 40 | 50 |
60 |
70 |
|
| Ubucucike (g / cm3) | 1.01 | 1.01 | 1.01 | 1.01 | 1.01 | |
| Imbaraga zingana (MPa) | 4.0 |
4.5 |
6.0 |
7.0 |
8.0 |
|
| Kurambura (%) | 150 | 170 | 220 | 150 | 80 |
|
| Amarira amarira (kN / m) | 12 | 14 | 20 |
18 | 10 |
|
| Kugabanuka kumurongo (%) | 2.1 |
2.1 |
2.1 |
2.0 |
2.0 |
|
| Kohereza (%) | 94 |
94 |
94 |
94 |
94 |
|