LSR yezvigadzirwa zvemhando yepamusoro (LSR)

Chikumbiro: chakakodzera kugadzira LED package, eyegirazi inobata, earphonesleeve, nezvimwe.
Zvinhu zvinokosha: kujeka kwepamusoro, simba guru.
  • GA-2230

  • Herchy

Kuwanikwa:
Huwandu:

Muedzo: A/B reshiyo ye1 :1, 130°C x 5min x 15MPa.

Product parameters
Product GA-2230 GA-2240 GA-2250 GA-2260 GA-2270
Chitarisiko Transparent
Viscosity(Pa.s)
10 10 8 5 5
Kuoma (ShoreA) 30 40 50
60
70
Density(g/cm3) 1.01 1.01 1.01 1.01 1.01
Tensile simba (MPa) 4.0
4.5
6.0
7.0
8.0
Elongation(%) 150 170 220 150 80
Simba rekubvarura (kN/m) 12 14 20
18 10
Linear shrinkage(%) 2.1
2.1
2.1
2.0
2.0
Transmittance(%) 94
94
94
94
94











Zvakapfuura: 
Zvinotevera: 

KUKURUMIDZA ZVINONYANYA

ZVINHU ZEDU

CONTACT INFORMATION

Wedzera: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |   Privacy Policy | Support By Leadong.