LSR for super transparent products (LSR)

Ntchito: oyenera kupanga phukusi LED, chofukizira diso, earphonesleeve, etc.
Zofunikira zazikulu: kuwonekera kwakukulu, mphamvu yayikulu.
  • GA-2230

  • Herchy

kupezeka:
kuchuluka:

Mayeso: Chiŵerengero cha A/B cha 1 :1, 130°C x 5min x 15MPa.

Zogulitsa katundu
Zogulitsa GA-2230 GA-2240 GA-2250 GA-2260 GA-2270
Maonekedwe Zowonekera
Viscosity (Pa.s)
10 10 8 5 5
Kuuma (ShoreA) 30 40 50
60
70
Kachulukidwe (g/cm3) 1.01 1.01 1.01 1.01 1.01
Mphamvu yamagetsi (MPa) 4.0
4.5
6.0
7.0
8.0
Elongation(%) 150 170 220 150 80
Mphamvu yamisozi (kN/m) 12 14 20
18 10
Kuchepa kwa mzere (%) 2.1
2.1
2.1
2.0
2.0
Kutumiza (%) 94
94
94
94
94











Zam'mbuyo: 
Ena: 

MALANGIZO OPHUNZITSA

ZOPHUNZITSA ZATHU

ZAMBIRI ZAMALUMIKIZIDWE

Onjezani: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Ufulu     2023 Shanghai Herchy Rubber Co., Ltd. Mapu atsamba |   Mfundo Zazinsinsi | Support By Leadong.