LSR bakeng sa lihlahisoa tse hlakileng haholo (LSR)

Kopo: e loketse ho hlahisa sephutheloana sa LED, sets'oants'o sa likhalase tsa mahlo, lesela la li-earphone, joalo-joalo.
Lintlha tse ka sehloohong: pepeneneng e phahameng, matla a phahameng.
  • GA-2230

  • Herchy

Boteng:
Bongata:

Teko: Karo-karolelano ea A/B ea 1 :1, 130°C x 5min x 15MPa.

Lihlahisoa tsa lihlahisoa
Sehlahisoa GA-2230 GA-2240 GA-2250 GA-2260 GA-2270
Ponahalo Tse pepeneneng
Viscosity(Pa.s)
10 10 8 5 5
Ho thatafala (LebopoA) 30 40 50
60
70
Boima ba 'mele(g/cm3) 1.01 1.01 1.01 1.01 1.01
Tensile Matla (MPa) 4.0
4.5
6.0
7.0
8.0
Elongation(%) 150 170 220 150 80
Matla a ho lla (kN/m) 12 14 20
18 10
Ho honyela ha mola(%) 2.1
2.1
2.1
2.0
2.0
Phetiso(%) 94
94
94
94
94











E fetileng: 
E 'ngoe: 

LIEKETSENG POTLAKO

LIHLAHISO TSA RONA

MOKHOA OA PUISANO

Eketsa: No.33, Lane 159, Taiye Road, Setereke sa Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Sebaka sa marang-rang |   Leano la Lekunutu | Tšehetso Ka Leadong.