LSR fun awọn ọja ti o han gbangba (LSR)

Ohun elo: o dara fun iṣelọpọ package LED, dimu gilasi oju, apo eti, bbl
Key awọn ẹya ara ẹrọ: ga akoyawo, ga agbara.
  • GA-2230

  • Herchy

Wiwa:
Opoiye:

Idanwo: Ipin A/B ti 1: 1, 130°C x 5min x 15MPa.

Ọja sile
Ọja GA-2230 GA-2240 GA-2250 GA-2260 GA-2270
Ifarahan Sihin
Igi (Pa.s)
10 10 8 5 5
Lile ( ShoreA) 30 40 50
60
70
Ìwúwo (g/cm3) 1.01 1.01 1.01 1.01 1.01
Agbara fifẹ (MPa) 4.0
4.5
6.0
7.0
8.0
Ilọsiwaju(%) 150 170 220 150 80
Agbara omije (kN/m) 12 14 20
18 10
Idinku laini (%) 2.1
2.1
2.1
2.0
2.0
Gbigbe(%) 94
94
94
94
94











Ti tẹlẹ: 
Itele: 

Awọn ọna asopọ kiakia

Awọn ọja WA

IBI IWIFUNNI

Fi kun: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tẹli / WhatsApp / Skype: +86 15221953351
Aṣẹ-lori-ara     2023 Shanghai Herchy Rubber Co., Ltd. maapu aaye |   Asiri Afihan | Atilẹyin Nipasẹ Leadong.