GA-2230
Herchy
| kasedhiyan: | |
|---|---|
| Jumlah: | |
~!phoenix_var120!~
| Parameter produk | ||||||
| produk | GA-2230 | GA-2240 | GA-2250 | GA-2260 | GA-2270 | |
| Penampilan | Transparan | |||||
| Viskositas (Pa) |
10 | 10 | 8 | 5 | 5 | |
| Kekerasan (ShoreA) | 30 | 40 | 50 |
60 |
70 |
|
| Kapadhetan (g/cm3) | 1.01 | 1.01 | 1.01 | 1.01 | 1.01 | |
| Kekuatan tarik (MPa) | 4.0 |
4.5 |
6.0 |
7.0 |
8.0 |
|
| Elongasi (%) | 150 | 170 | 220 | 150 | 80 |
|
| Kekuwatan sobek (kN/m) | 12 | 14 | 20 |
18 | 10 |
|
| Penyusutan linear (%) | 2.1 |
2.1 |
2.1 |
2.0 |
2.0 |
|
| Transmisi (%) | 94 |
94 |
94 |
94 |
94 |
|