LSR ka ɲɛsin super transparent ka fɛnw ma (LSR) .

Aplikasi: a bɛnnen don ka LED pake dilan, ɲɛkisɛ minɛyɔrɔ,tulolanɛgɛ, wdfl.
Fɛn kolomaw: kɛnɛyako ka bon, fanga ka bon.
  • GA-2230 .

  • Herchy .

A sɔrɔli:
Hakɛ: .

Kɔrɔbɔli: A/B hakɛ 1 :1, 130°C x 5min x 15MPa.

Product Paramɛtɛrɛw .
Ka kɛ GA-2230 . GA-2240 ye GA-2250 . GA-2260 . GA-2270 .
Yecogo Jɛlen
Viscosité(Pa.s) ka .
10 10 8 5 5
Gɛlɛya (Shoaa) . 30 40 50
60
70
Densité(g/cm3) ye. 1.01 1.01 1.01 1.01 1.01
Sɛgɛsɛgɛli fanga (MPa) . 4.0
4.5
6.0
7.0
8.0
Janya(%) . 150 170 220 150 80
Ɲɛjibɔ fanga (KN/M) . 12 14 20
18 10
Rétrécissement linéaire(%) 1. Bamako, Mali. 2.1
2.1
2.1
2.0
2.0
transmittance(%) . 94
94
94
94
94











Tɛmɛnen: 
Nata: 

LINKS TELIKANW

An ka fɛn dilannenw .

KUNNAFONIW MINNU BƐ SƆRƆ

A farala: No.33, Lane 159, Taiye sira kan, Fengxian mara la, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Hakilila-jɔ-sɛbɛn     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap (yɔrɔ karti). |   Kunnafoni dogolenw ka sariya | Dɛmɛn By Leadong ye.