GA-8151P
Herchy
| Availability: | |
|---|---|
| Quantity: | |
Test: 1% of curing agent (50% paste of DBPMH ins小conegum), 175'C x 5min x 15MPa.
| Product parameters | ||||
| Product | GA-8151P |
GA-8161P | GA-8171P | GA-8181P |
| Appearance | White |
|||
| Williamplasticity |
210 |
255 |
300 |
340 |
| Hardness (ShoreA) |
50 |
60 |
70 |
80 |
| Density(g/cm3) | 1.35 |
1.45 |
1.45 |
1.48 |
| Tensile strength (MPa) |
6.0 |
6.0 |
6.0 |
5.5 |
| Elongation(%) | 380 |
280 |
200 |
200 |
| Tear strength (kN/m) | 14 |
13 |
13 |
12 |
| Flame retardant grade/2mm | V-0 |
|||