GA-81 × 1P Rubber-Silarda Rubber (2mm) (HCR)

Gusaba: bikwiranye no gukora ubwoko bwose bwibicuruzwa bya flame-retardant.
Ibintu byingenzi byingenzi: imbaraga nyinshi, halogen-flame flame 「etardant, flame retardancy, pass the authentication ya RoHS na REACH.
  • GA-8151P

  • Herchy

Kuboneka:
Umubare:

Ikizamini: 1% yumuti ukiza (50% paste ya DBPMH ins 小 conegum), 175'C x 5min x 15MPa.


Ibipimo byibicuruzwa
Ibicuruzwa GA-8151P
GA-8161P GA-8171P GA-8181P
Kugaragara Cyera
Yamamoto
210
255
300
340
Gukomera (ShoreA)
50
60
70
80
Ubucucike (g / cm3) 1.35
1.45
1.45
1.48
Imbaraga zingana (MPa)

6.0
6.0
6.0
5.5
Kurambura (%) 380
280
200
200
Amarira amarira (kN / m) 14
13
13
12
Icyiciro cya retardant urwego / 2mm                                  V-0









Mbere: 
Ibikurikira: 

LINKS

IBICURUZWA BYACU

AMAKURU

Ongeraho: No.33, Umuhanda 159, Umuhanda wa Taiye, Akarere ka Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Uburenganzira     2023 Shanghai Herchy Rubber Co., Ltd. Ikarita |   Politiki Yibanga | Inkunga Na Kurongora.