Tel: +86 15221953351 E-mail hmanga zawhfiah theih a ni. info@herchyrubber.com
Please Choose Your Language
PRODUCTS THIL THAWN THAWN THIL THIL THIL THIL THIL THIL THIL THIL THIL THAWN
Hetah hian i awm: In » Thil siam chhuah te » Synthesis Rubber hmanga siam a ni » VMQ Silicone hmanga siam a ni » GA-81×1P Meialh laka invenna Silicone Rubber (2mm) (HCR)

loading a ni

Share to:
facebook ah in share theih a ni
twitter hmanga share theih a ni
line insem theihna button a ni
wechat hmanga insem theihna button a ni
linkedin a insem theihna tur a ni
pinterest hmanga insem theihna button
whatsapp a insem theihna tur a ni
sharethih hi share theih a ni

GA-81×1P Meialh laka invenna Silicone Rubber (2mm) (HCR) hmanga siam a ni.

A hman dan: meialh laka invenna thil chi hrang hrang siamna atana tha.
Key features: chakna sang tak, halogen-free flame「etardant,meialh retardancy tha tak,RoHS leh REACH authentication pass.
  • GA-8151P ah a awm

  • Herchy a ni

A awm theihna:
A zat:

Test: Curing agent 1% (DBPMH ins小conegum paste 50%), 175’C x 5min x 15MPa.


Product parameter hrang hrang
Thilsiam GA-8151P ah a awm
GA-8161P ah a awm GA-8171P ah a awm GA-8181P ah a awm
Landan Var
Williamplasticity a ni
210
255
300
340
Hardness (ShoreA) a ni.
50
60
70
80
Density(g/cm3) a ni. 1.35
1.45
1.45
1.48
Tensile chakna (MPa) 1.1.

6.0
6.0
6.0
5.5
A sei zawng(%) . 380
280
200
200
Mittui tlak chakna (kN/m) . 14
13
13
12
Meialh laka invenna grade/2mm                                  V-0 a ni









Hma chiah: 
Dawtchiah: 

QUICK LINKS A AWM VE ANG

CONTACT THIL AWM DAN

Add: No.33, Lane 159, Taiye kawngpui, Fengxian District, Shanghai-a awm a ni
Tel / WhatsApp / Skype: +86 15221953351 ah zawhfiah theih a ni
E-mail hmangin:  info@herchyrubber.com
A rilru a hah lutuk   chuan a rilru   2023 a buai em em a. Shanghai Herchy Rubber Co., Ltd. Sitemap a ni |   Thuruk humhalh dan tur | Support By Leadong a ni.