| Hoeveelheid: | |
Toets: 1% genesingsmiddel (50% pasta van DBPMH ins小conegum), 175'C x 5min x 15MPa.
| Produk parameters | ||||
| Produk | GA-8151P |
GA-8161P | GA-8171P | GA-8181P |
| Voorkoms | Wit |
|||
| Williamplastisiteit |
210 |
255 |
300 |
340 |
| Hardheid (ShoreA) |
50 |
60 |
70 |
80 |
| Digtheid (g/cm3) | 1.35 |
1.45 |
1.45 |
1.48 |
| Treksterkte (MPa) |
6.0 |
6.0 |
6.0 |
5.5 |
| Verlenging (%) | 380 |
280 |
200 |
200 |
| Skeursterkte (kN/m) | 14 |
13 |
13 |
12 |
| Vlamvertrager graad/2mm | V-0 |
|||