GA-81×1P Caoutchouc de silicone oyo epekisaka mɔtɔ (2mm) (HCR)

Kosalela: ebongi mpo na kobimisa biloko ya ndenge nyonso oyo epekisaka mɔtɔ.
Makambo ya ntina: makasi ya likolo, halogène-free flamme「etardant,excellente flamme retardancy,lekisa authentification ya RoHS mpe REACH.
  • GA-8151P

  • HERCHY .

Bozali:
Motango:

Momekano: 1% ya agent curing (50% ya pâte ya DBPMH ins小conegum), 175'C x 5min x 15MPa.


Ba paramètres ya produit
Eloko GA-8151P
GA-8161P. Ezali na ntina mingi GA-8171P. Ezali na ntina mingi GA-8181P. Ezali na ntina mingi
Komonana Mpembe
Williamplasticité ya kosala
210
255
300
340
Bokasi ya makasi (ShoreA) .
50
60
70
80
Densité(g/cm3) Ezali na ba . 1.35
1.45
1.45
1.48
Bokasi ya kokangama (MPa) .

6.0
6.0
6.0
5.5
Elongation(%) ya . 380
280
200
200
Bokasi ya kopasola (kN/m) . 14
13
13
12
Grade retardant ya mɔ́tɔ/2mm                                  V-0









Oyo eleki: 
Oyo elandi: 

BA LIEN YA NOKI

BILOKO NA BISO

BA INFORMATIONS YA CONTACT

Bakisa: No.33, Nzela 159, Nzela ya Taiye, District ya Fengxian, Shanghai
Tel / Whatsapp / Skype: +86 15221953351