GA-81×1P Dab-Cusub Silikoon ah (2mm) (HCR)

Codsiga: ku habboon soo saarista dhammaan noocyada alaabooyinka ololka-celiska ah.
Astaamaha muhiimka ah: xoog sare, olol aan halogen-free 「Etardant, dib u dhac ololka heer sare ah, gudub aqoonsiga RoHS iyo REACH.
  • GA-8151P

  • Herchy

Helitaanka:
Tirada:

Tijaabada: 1% ee wakiilka daawaynta (50% koollada DBPMH ins小conegum), 175'C x 5min x 15MPa.


Xuduudaha alaabta
Alaabta GA-8151P
GA-8161P GA-8171P GA-8181P
Muuqashada Caddaan
Williamplasticity
210
255
300
340
Adag ( ShoreA)
50
60
70
80
Cufnaanta (g/cm3) 1.35
1.45
1.45
1.48
Xoog xajin (MPa)

6.0
6.0
6.0
5.5
Dheeraynta(%) 380
280
200
200
Xoogga jeexjeexa (kN/m) 14
13
13
12
Darajada ololka/2mm                                  V-0









Kii hore: 
Xiga: 

XIDHIIDHYADA DEGDEGGA AH

Alaabooyinkayaga

MACLUUMAADKA XIRIIRKA

Kudar: No.33, Lane 159, Wadada Taiye, Degmada Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Xuquuqda daabacaadda     2023 Shanghai Herchy Rubber Co., Ltd. Khariidadda goobta |   Siyaasadda Qarsoonnimada | Taageerada By Leadong.