GA-8151P na ɛwɔ hɔ
Herchy a ɔyɛ ɔbarima
| Nea Ɛwɔ Hɔ: | |
|---|---|
| Dodow: | |
Sɔhwɛ: 1% a ɛyɛ aduru a wɔde sa yare (50% a wɔde ahyɛ DBPMH ins小conegum mu), 175'C x 5min x 15MPa.
| Nneɛma a wɔyɛ no parameters | ||||
| Adwadeɛ | GA-8151P na ɛwɔ hɔ |
GA-8161P na ɛwɔ hɔ | GA-8171P na ɛwɔ hɔ | GA-8181P na ɛwɔ hɔ |
| Mmaeɛ | Fitaa |
|||
| Williamplasticity a wɔde yɛ nneɛma |
210 |
255 |
300 |
340 |
| Nneɛma a ɛyɛ den (ShoreA) . |
50 |
60 |
70 |
80 |
| Nsuo a ɛyɛ den(g/cm3) . | 1.35 |
1.45 |
1.45 |
1.48 |
| Ahoɔden a wɔde twe ade (MPa) . |
6.0 |
6.0 |
6.0 |
5.5 |
| Ntrɛwmu(%) . | 380 |
280 |
200 |
200 |
| Ahoɔden a ɛtetew mu (kN/m) . | 14 |
13 |
13 |
12 |
| Ogya a ɛmma ogya ntumi nkɔ mu grade/2mm | V-0 |
|||