Okugezesa: Omugerageranyo gwa A/B ogwa 1 :1, 130°C x 5min x 15MPa
| Ebipimo by'ebintu . | |||||
| Ekyamaguzi | GA-2135-15 | GA-2135-25 | GA-2135-35 | GA-2135-45 | |
| Endabika | Translucent . | ||||
| Obuziba(Pa.s) . |
60 | 30 | 38 | 30 | |
| Obukakanyavu (Shorea) . | 18 | 26 | 35 |
48 |
|
| Densite(g/cm3) . | 1.03 |
1.06 | 1.06 | 1.10 | |
| Amaanyi g’okusika (MPA) . | 2.5 |
2.8 |
4.2 |
5.5 |
|
| okuwanvuwa(%) . | 400 | 380 | 330 | 250 | |
| Amaanyi g’okukutuka (kn/m) . | 8 | 9.5 | 11.5 |
16 | |
| Okukendeera kw’ennyiriri(%) . | 1.7 | 1.7 | 1.7 | 1.7 | |