GA-2135
Herchy
| Dobavljivost: | |
|---|---|
| Količina: | |
Test: razmerje A/B 1:1, 130 °C x 5 min x 15 MPa
| Parametri izdelka | |||||
| Izdelek | GA-2135-15 | GA-2135-25 | GA-2135-35 | GA-2135-45 | |
| Videz | Prosojno | ||||
| Viskoznost (Pa.s) |
60 | 30 | 38 | 30 | |
| Trdota (ShoreA) | 18 | 26 | 35 |
48 |
|
| Gostota (g/cm3) | 1.03 |
1.06 | 1.06 | 1.10 | |
| Natezna trdnost (MPa) | 2.5 |
2.8 |
4.2 |
5.5 |
|
| Raztezek (%) | 400 | 380 | 330 | 250 | |
| Trdna trdnost (kN/m) | 8 | 9.5 | 11.5 |
16 | |