GA-2135 LSR ka ɲɛsin Pad sɛbɛnni ma (LSR) .

A kɛcogo: a bɛnnen don ka pad imprimante kunkolo dilan, suguya caman ofmolds. 
Fɛn kolomaw: furakɛli so funteni na, debubbling ɲuman ani masin nafa.
  • GA-2135 ye

  • Herchy (Herchy) ye

A sɔrɔli:
Hakɛ: .

Kɔrɔbɔli : A/B hakɛ ye 1 :1 ye, 130°C x 5min x 15MPa


Fɛn dilannenw ka paramɛtiriw
Ka kɛ GA-2135-15 kɔnɔ GA-2135-25 kɔnɔ GA-2135-35 kɔnɔ GA-2135-45 kɔnɔ
Yecogo Translucent (yɔrɔ jɛlen) ye
Viscosité(Pa.s) ka .
60 30 38 30
Gɛlɛya (KɔgɔjidaA) . 18 26 35
48
Densité(g/cm3) ye.

1.03

1.06 1.06 1.10
Sɛgɛsɛgɛli fanga (MPa) . 2.5
2.8
4.2
5.5
Janya(%) . 400 380 330 250
Ɲɛjibɔ fanga (kN/m) . 8 9.5 11.5
16
Linearshrinkage(%) Bamako, Mali. 1.7 1.7 1.7 1.7








Tɛmɛnen: 
Nata: 

LINKS TELIKANW

AN KA FƐƐRƐW

KUNNAFONIW MINNU BƐ SƆRƆ

A farala: No.33, Lane 159, Taiye sira kan, Fengxian mara la, Shanghai
Telefɔni / WhatsApp / Skype: +86 15221953351
Hakilila-jɔ-sɛbɛn     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap (yɔrɔ karti). |   Kunnafoni dogolenw ka sariya | Dɛmɛn By Leadong ye.