GA-2135 LSR for Pad Printing (LSR)

Application: suitable for producing pad printing head, various kinds ofmolds. 
Key features: curing at room temperature, excellent debubbling andmechanical property.
  • GA-2135

  • Herchy

Availability:
Quantity:

Test: A/B ratio of 1 :1, 130°C x 5min x 15MPa


Product parameters
ProductGA-2135-15GA-2135-25GA-2135-35GA-2135-45
AppearanceTranslucent
Viscosity(Pa.s)
60303830
Hardness (ShoreA)182635
48
Density(g/cm3)

1.03

1.061.061.10
Tensile strength (MPa)2.5
2.8
4.2
5.5
Elongation(%)400380330250
Tear strength (kN/m)89.511.5
16
Linearshrinkage(%)1.71.71.71.7








Previous: 
Next: 

QUICK LINKS

OUR PRODUCTS

CONTACT INFORMATION

Add: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +8615221953351
Copyright  2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |  Privacy Policy | Support By Leadong.