Ulapha: Ikhaya » Imikhiqizo » Irabha Yokuhlanganisa » I-Silicone ye-VMQ GA -2135 LSR for Pad Printing (LSR)

iyalayisha

Yabelana ku-:
inkinobho yokwabelana ye-facebook
inkinobho yokwabelana ye-twitter
inkinobho yokwabelana ngomugqa
inkinobho yokwabelana ye-wechat
inkinobho yokwabelana ye-linkedin
inkinobho yokwabelana ye-pinterest
inkinobho yokwabelana ye-whatsapp
yabelana ngale nkinobho yokwabela

I-GA-2135 LSR for Pad Printing (LSR)

Isicelo: ilungele ukukhiqiza ikhanda lokuphrinta lephedi, izinhlobo ezahlukahlukene zokubunjwa. 
Izici eziyinhloko: ukuphulukisa ekamelweni lokushisa, ukulungiswa okuhle kakhulu kanye nempahla yemishini.
  • GA-2135

  • I-Herchy

Ukutholakala:
Ubuningi:

Isivivinyo: A/B isilinganiso 1 :1, 130°C x 5min x 15MPa


Imingcele yomkhiqizo
Umkhiqizo GA-2135-15 GA-2135-25 GA-2135-35 GA-2135-45
Ukubukeka I-Translucent
I-Viscosity(Pa.s)
60 30 38 30
Ukuqina (ShoreA) 18 26 35
48
Ukuminyana(g/cm3)

1.03

1.06 1.06 1.10
Amandla e-Tensile (MPa) 2.5
2.8
4.2
5.5
Ubude(%) 400 380 330 250
Amandla wezinyembezi (kN/m) 8 9.5 11.5
16
Ukuncipha komugqa(%) 1.7 1.7 1.7 1.7








Okwedlule: 
Olandelayo: 

IZIXHUMANISI EZISHESHAYO

IMIKHIQIZO YETHU

ULWAZI LOKUXHUMANA

Engeza: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Ucingo / WhatsApp / Skype: +86 15221953351
I-imeyili:  info@herchyrubber.com
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Imephu yesayithi |   Inqubomgomo Yobumfihlo | Sekela Ngu I-Leadong.