GA-2135
Herchy
| Beschikbaarheid: | |
|---|---|
| Aantal: | |
Test: A/B-verhouding van 1:1, 130°C x 5min x 15MPa
| Productparameters | |||||
| Product | GA-2135-15 | GA-2135-25 | GA-2135-35 | GA-2135-45 | |
| Verschijning | Doorschijnend | ||||
| Viscositeit (Pa.s) |
60 | 30 | 38 | 30 | |
| Hardheid (ShoreA) | 18 | 26 | 35 |
48 |
|
| Dichtheid (g/cm3) | 1.03 |
1.06 | 1.06 | 1.10 | |
| Treksterkte (MPa) | 2.5 |
2.8 |
4.2 |
5.5 |
|
| Verlenging (%) | 400 | 380 | 330 | 250 | |
| Scheursterkte (kN/m) | 8 | 9.5 | 11.5 |
16 | |
| Lineaire krimp (%) | 1.7 | 1.7 | 1.7 | 1.7 | |