Ulapha: Ikhaya » Imikhiqizo » Irabha Yokuhlanganisa » I-FVMQ Fluorosilicone » Fluorosilicone Rubber FV9400

iyalayisha

Yabelana ku-:
inkinobho yokwabelana ye-facebook
inkinobho yokwabelana ye-twitter
inkinobho yokwabelana ngomugqa
inkinobho yokwabelana ye-wechat
inkinobho yokwabelana ye-linkedin
inkinobho yokwabelana ye-pinterest
inkinobho yokwabelana ye-whatsapp
yabelana ngale nkinobho yokwabelana

I-Fluorosilicone Rubber FV9400

Lo mkhiqizo uyingxube ye-homogeneous ye-fluorosilicone elastomer njengeglue eyisisekelo nama-filler ahlukahlukene kanye nezithasiselo.
Inamandla aphezulu kanye nokuqina.
Ukumelana nowoyela okuhle kakhulu, ukumelana ne-solvent kanye nokumelana nokushisa okuphezulu nokuphansi.
  • FV9400

  • I-Herchy

Ukutholakala:
Ubuningi:


Izinto

Izinkomba

Amabanga

FV9430

FV9440

FV9450

I-FV9460

FV9470

FV9480

Ukubukeka
Izindlela Zokuhlola

I-Milky white translucent

Okuphuzi

I-Gravity ethize/g/cm3

I-ASTM D792

1.38

1.41

1.42

1.43

1.45

1.47

Ukuqina/uguA

I-ASTM D2240

28

40

48

60

70

80

Amandla Okuqina/MPa

I-ASTM D412

10.2

9.5

9.5

10.2

9.9

8.1

I-Elongation At Break /%

I-ASTM D412

485

494

363

296

241

159

Amandla Ezinyembezi/KN/m

I-ASTM D624-B

18

26

19

22

21

16

Isethi Yokucindezela (177℃*22h)

I-ASTM D395

9

8

8

7

8

9

Ukuqina/%

I-ASTM D1054

41

35

46

40

37

39

*I-Heat Resistance
225℃×72h

Ukushintsha kokuqina/ugu A

+2

+2

+3

+2

+2

+3

Ukushintsha kwamandla okuqina,%

-18

-17

-21

-25

-20

-19

Ukwelula ngesikhathi sokushintsha kwekhefu, %

-19

-16

-18

-21

-16

-15

I-Fuel C

Ukushintsha Kwevolumu/%

23℃/72h

I-ASTM D471

+22

+19

+18

+19

+19

+19

Isimo Sokwelapha

Engeza izingxenye ezingu-0.7 ze-bis(2+5), i-vulcanisation eyodwa yesiteji 170℃×15min, i-vulcanisation yesiteji ezimbili: 200℃×4h.

Izenzo ezinconyiwe:


Kuphakanyiswe ukuthi kusetshenziswe ingxenye engu-0.6 ukuya ku-1 ye-ejenti yamakhemikhali ye-bisdipenta ukuze kutholakale i-vulcanization (2,5-dimethyl-2,5-bis(tert-butylperoxy)hexane).


Amakhasimende kufanele akhethe izinga lokushisa elifanele kakhulu nesikhathi sokwelapha ngokusekelwe kusayizi womkhiqizo kanye nendlela yokwelapha.


Ukupakishwa komkhiqizo:


Lo mkhiqizo awuyona ingozi, kunalokho wakhiwe nge-cardstock, ipulasitiki, namakhilogremu angu-10 esikhwameni ngasinye, izikhwama ezingu-2 ibhokisi ngalinye.


Iminyaka yokugcina:


Lo mkhiqizo unamandla okugeleza okubandayo, isikhwama kufanele sigwenywe ukuze singalimazi ngesikhathi sokuthutha noma ukusetshenziswa.


Gcina endaweni epholile, eyomile eneshalofu impilo yezinyanga eziyi-12.


Okwedlule: 
Olandelayo: 

IZIXHUMANISI EZISHESHAYO

IMIKHIQIZO YETHU

ULWAZI LOKUXHUMANA

Engeza: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Ucingo / WhatsApp / Skype: +86 15221953351
I-imeyili:  info@herchyrubber.com
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Imephu yesayithi |   Inqubomgomo Yobumfihlo | Sekela Ngu I-Leadong.