I-Fluoroelastomer -FKM/FPM

I-Fluoroelastomer iyi-polymer elastomer yokwenziwa equkethe ama-athomu e-fluorine kuma-athomu ekhabhoni eketango eliyinhloko noma iketango laseceleni. Ukwethulwa kwama-athomu e-fluorine kunikeza irabha ukumelana nokushisa okuhle kakhulu, ukumelana ne-oxidation, ukumelana nowoyela, ukumelana nokugqwala kanye nokumelana nokuguga komkhathi, futhi isetshenziswa kabanzi ku-aerospace, izindiza, izimoto, uphethiloli kanye nezinto zikagesi zasendlini.
Ukutholakala:
Ubuningi:

I-Fluoroelastomer rubber compound-FKM


Imikhiqizo yenjoloba ye-FKM inokumelana okuhle kakhulu nokushisa okuphezulu, ukumelana nokugqwala kwamakhemikhali, ukumelana nowoyela, ukusebenza okuhle kokuguquguquka okuhlala njalo, ukumelana nelangabi kanye nokungena kwegesi.


I-Fluoroelastomer isetshenziswa kakhulu ekubekweni uphawu kwezinga lokushisa eliphezulu neliphansi, i-vacuum instrumentation kanye nemishini, okokusebenza kwamakhemikhali, imoto, izindiza kanye neminye imikhakha.


I-Herchy Rubber ineqembu lochwepheshe le-R&D ukuze lihlangabezane nezidingo zokwenza ngokwezifiso zamakhasimende ethu.

●Isistimu ye-bisphenol vulcanization kanye nesistimu ye-peroxide vulcanization

● Thuthukisa futhi ukhiqize imikhiqizo yokubumba, umjovo, i-extrusion nezinye izindlela zokucubungula.

●Enza ngendlela oyifisayo inhlanganisela ye-fluoroelastomer enobunzima obungu-50-90 degrees, imibala ehlukahlukene kanye nezinhlelo zokusebenza ngokuvumelana nezidingo zamakhasimende.


I-Herchy Uhlobo lwe-Vulcanization Okuqukethwe kwe-fluorine I-Money viscosity Ukuminyana Amandla aqinile Ukwandisa ngesikhathi sekhefu I-TR10 Isethi yokucindezela Isicelo Umlingiswa







200℃*72h ASTM D395 Uhlobo B
Ibanga % I-ML(1+10)121℃ g/cm3 Mpa % %
I-FKM-65B20 I-bisphenol 65.9 20 1.8 12.3 170 -17 17 O-izindandatho; Gasket Isethi yokucindezela ephansi;
I-liquidity enhle;
I-FKM-65B40 I-bisphenol 65.9 40 1.81 14.3 180 -17 16 O-izindandatho; Gasket Amandla emishini ephezulu;
Isethi yokucindezela okuphansi
I-FKM-65B60 I-bisphenol 65.9 60 1.81 15.5 180 -17 16 O-izindandatho; Gasket Amandla emishini ephezulu;
Isethi yokucindezela okuphansi
I-FKM-68B40 I-bisphenol 68.5 40 1.85 14.3 220 -14 26 O-izindandatho; Gasket I-liquidity enhle;
Ukumelana okuhle kakhulu kwemidiya yamakhemikhali;
ukumelana nokushisa okuphezulu
I-FKM-68B60 I-bisphenol 68.5 60 1.85 16.2 200 -14 26 O-izindandatho; Gasket Amandla aphezulu mechanical;
Ukumelana Excellent kwabezindaba amakhemikhali;
Ukushisa okuphezulu ukumelana
I-FKM-65B30S I-bisphenol 65.9 30 1.80 15.0 190 -20 21 Imikhiqizo enwetshiwe, imikhiqizo ejovwe, imikhiqizo ebunjiwe Ukumelana nokushisa okuphansi;
Amandla aphezulu mechanical;
liquidity Good;
I-FKM-70P30 I-Peroxide 70 30 1.9 18.5 220 -7 36 Imikhiqizo enwetshiwe, imikhiqizo ejovwe, imikhiqizo ebunjiwe I-liquidity enhle;
Ukumelana okuhle kwe-asidi ne-alkali;
Ukumelana okuhle kakhulu kwemidiya yamakhemikhali;
ukumelana nokushisa okuphezulu
I-FKM-68P45 I-Peroxide 68 45 1.85 16.5 280 -16 36 Imikhiqizo enwetshiwe, imikhiqizo ejovwe, imikhiqizo ebunjiwe I-liquidity enhle;
Ukumelana okuhle kwe-asidi ne-alkali;
Ukumelana okuhle kakhulu kwemidiya yamakhemikhali;
ukumelana nokushisa okuphezulu


1.Seal

Isigxivizo senjini

Uphawu lwami

Chemical seal

I-Superheated steam seal

Iwashi le-valve seal

Isitsha sesikhumba

Uwoyela uphawu


2. Ipayipi

Ipayipi lerabha lokushisa eliphezulu

Ipayipi le-automobile fuel

Ipayipi lamafutha endiza

Ipayipi elihlangene likathayela


3. Izintambo nezintambo

Intambo nekhebuli eyenziwe nge-fluoroelastomer igobeka kahle futhi inezici ezinhle zokuvikela


4. Fiberglass tape

Ukushisa okuphezulu kwe-300 ℃ kanye nokumelana nokugqwala kwamakhemikhali


Okwedlule: 
Olandelayo: 

IZIXHUMANISI EZISHESHAYO

IMIKHIQIZO YETHU

ULWAZI LOKUXHUMANA

Engeza: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Ucingo / WhatsApp / Skype: +86 15221953351
I-imeyili:  info@herchyrubber.com
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Imephu yesayithi |   Inqubomgomo Yobumfihlo | Sekela Ngu I-Leadong.