Fluorosilicone rhaba FV9400 .

Xiendliwa lexi i nkatsakanyo wa homogeneous wa fluorosilicone elastomer tani hi base glue na ti fillers to hambana hambana na swiengeteri.
Yina matimba yale henhla xikan’we naku tiyisela.
Ku tiya ka kahle swinene ka oyili, ku tiya ka solvent xikan’we naku tiya ka mahiselo yale henhla nale hansi.
  • FV9400

  • Herchy

Ku kumeka:
Nhlayo: .


Swilo

Swikombiso

Tigredi

FV9430

FV9440

FV9450

FV9460

FV9470

FV9480

xa ku languteka
Maendlelo ya Xikambelo

Milky white yi vonaka kahle

Xihlovo xo tshwuka

Nkoka wo karhi/ g/cm3

ASTM D792

1.38

1.41

1.42

1.43

1.45

1.47

Ku tiya/ribuwaA

ASTM D2240 ya xirhendzevutani

28

40

48

60

70

80

Ku tiya ka ku tsana/MPa

ASTM D412

10.2

9.5

9.5

10.2

9.9

8.1

Ku Elongation Hi Nkarhi wo Pfumala /% .

ASTM D412

485

494

363

296

241

159

Matimba ya ku handzuka/KN/m

ASTM D624-B ya xirhendzevutani

18

26

19

22

21

16

Seti ya Ntshikelelo(177°C * 22h)

ASTM D395

9

8

8

7

8

9

Sihalala/%

ASTM D1054

41

35

46

40

37

39

*Ku tiya ka ku hisa
225°C×72h

Ku cinca ka ku tiya /shore A

+2

+2

+3

+2

+2

+3

Ku cinca ka matimba ya ku tsana, % .

-18

-17

-21

-25

-20

-19

Ku leha eka ku cinca ka break, % .

-19

-16

-18

-21

-16

-15

Mafurha ya C

Ku Cinca ka Vholumo/% .

23°C/72h

ASTM D471

+22

+19

+18

+19

+19

+19

Xiyimo xo Horisa

Engeta 0.7 wa swiphemu swa bis(2+5), vulcanisation ya xiteji xin’we 170°C×15min, vulcanisation ya switeji swimbirhi: 200°C×4h.

Swiendlo leswi ringanyetiweke:


Swi ringanyetiwa ku tirhisa 0.6 kuya eka 1 wa xiphemu xa bisdipenta chemical agent eka vulcanization (2,5-dimethyl-2,5-bis(tert-butylperoxy)hexane).


Vaxavi vafanele ku hlawula mahiselo lawa ya faneleke swinene na nkarhi wo horisa kuya hi vukulu bya xiendliwa xikan’we na ndlela yo horisa.


Ku pakiwa ka swikumiwa:


Xiendliwa lexi a xi na khombo, ematshan’wini ya sweswo xi vumbiwa hi khadi, pulasitiki, na 10 wa tikhilogiramu hi nkwama, 2 wa minkwama hi bokisi.


Malembe ya vuhlayiselo: .


Xiendliwa lexi xina vuswikoti byo khuluka hi xirhami, nkwama wufanele ku papalatiwa leswaku wunga onhaki loko wu fambisiwa kumbe kutirhisiwa.


Hlayisa eka ndzhawu yo kufumela, yo oma leyingana vutomi bya 12 wa tinhweti.


Endzhaku: 
Landzelaka: 

XITLHOKOVETSELO XA XITLHANYI

SWILO SWA HINA

VUXOKOXOKO BYA VUXOKOXOKO

Engetelani: No.33, Lane 159, Gondzo ra Taiye, Xifundzha xa Fengxian, Shanghai
Riqingho / WhatsApp / Skype: +86 15221953351
Vukorhokeri bya Vutshila     2023 Shanghai Herchy Rubber Co., Ltd. Mepe wa sayiti |   Pholisi ya Vuhlayiseki | Nseketelo Hi Leadong.