FV9400
Herchy
| Availability: | |
|---|---|
| Dami: | |
Mga bagay |
Mga tagapagpahiwatig |
||||||
Mga grado |
FV9430 |
FV9440 |
FV9450 |
FV9460 |
FV9470 |
FV9480 |
|
sa Hitsura |
Milky white translucent |
Madilaw-dilaw |
|||||
Specific Gravity/ g/cm3 |
ASTM D792 |
1.38 |
1.41 |
1.42 |
1.43 |
1.45 |
1.47 |
Katigasan/baybayinA |
ASTM D2240 |
28 |
40 |
48 |
60 |
70 |
80 |
Lakas ng makunat/MPa |
ASTM D412 |
10.2 |
9.5 |
9.5 |
10.2 |
9.9 |
8.1 |
Pagpahaba Sa Break /% |
ASTM D412 |
485 |
494 |
363 |
296 |
241 |
159 |
Lakas ng Pagkapunit/KN/m |
ASTM D624-B |
18 |
26 |
19 |
22 |
21 |
16 |
Compression Set(177℃*22h) |
ASTM D395 |
9 |
8 |
8 |
7 |
8 |
9 |
Katatagan/% |
ASTM D1054 |
41 |
35 |
46 |
40 |
37 |
39 |
*Heat Resistance |
Pagbabago ng katigasan / baybayin A |
+2 |
+2 |
+3 |
+2 |
+2 |
+3 |
Pagbabago ng lakas ng makunat, % |
-18 |
-17 |
-21 |
-25 |
-20 |
-19 |
|
Pagpahaba sa pagbabago ng break, % |
-19 |
-16 |
-18 |
-21 |
-16 |
-15 |
|
gasolina C Pagbabago ng Dami/% 23℃/72h |
ASTM D471 |
+22 |
+19 |
+18 |
+19 |
+19 |
+19 |
Kundisyon ng Paggamot |
Magdagdag ng 0.7 bahagi ng bis(2+5), isang yugto ng bulkanisasyon 170℃×15min, dalawang yugto ng bulkanisasyon: 200℃×4h. |
||||||
Mga inirerekomendang aksyon:
Iminumungkahi na gumamit ng 0.6 hanggang 1 bahagi ng bisdipenta chemical agent para sa vulcanization (2,5-dimethyl-2,5-bis(tert-butylperoxy)hexane).
Dapat piliin ng mga customer ang pinakaangkop na temperatura at oras para sa paggamot batay sa laki at paraan ng paggamot ng produkto.
Packaging ng produkto:
Ang produktong ito ay hindi mapanganib, sa halip ay binubuo ito ng cardstock, plastic, at 10 kilo bawat bag, 2 bag bawat kahon.
Edad ng imbakan:
Ang produktong ito ay may kapasidad ng malamig na daloy, dapat na iwasan ang bag upang hindi ito masira sa panahon ng transportasyon o paggamit.
Panatilihin sa isang cool, tuyo na kapaligiran na may shelf life na 12 buwan.