Fluorosilicon Rubber FV9400

Wannan samfurin shine cakuda mai kama da fluorosilicone elastomer azaman manne tushe da filaye daban-daban da ƙari.
Yana da babban ƙarfi da juriya.
Kyakkyawan juriya mai, juriya mai ƙarfi da juriya mai ƙarfi da ƙarancin zafin jiki.
  • Saukewa: FV9400

  • Herchy

samuwa:
Yawan:


Abubuwa

Manuniya

Maki

Saukewa: FV9430

Saukewa: FV9440

Saukewa: FV9450

Saukewa: FV9460

Saukewa: FV9470

Saukewa: FV9480

Bayyanawa
Hanyoyin Gwajin

Milky farin translucent

Rawaya

Takamaiman nauyi/g/cm3

Saukewa: ASTM D792

1.38

1.41

1.42

1.43

1.45

1.47

Hardness/hardA

Saukewa: ASTM D2240

28

40

48

60

70

80

Ƙarfin Ƙarfin Ƙarfi / MPA

Saukewa: ASTM D412

10.2

9.5

9.5

10.2

9.9

8.1

Tsawaita Lokacin Hutu /%

Saukewa: ASTM D412

485

494

363

296

241

159

Ƙarfin Hawaye/KN/m

Saukewa: ASTM D624-B

18

26

19

22

21

16

Saitin matsawa (177 ℃ * 22h)

Saukewa: ASTM D395

9

8

8

7

8

9

Juriya/%

Saukewa: ASTM D1054

41

35

46

40

37

39

* Resistance Heat
225 ℃ × 72h

Canjin taurin/hardness A

+2

+2

+3

+2

+2

+3

Canjin ƙarfin ƙarfi, %

-18

-17

-21

-25

-20

-19

Tsawaitawa a canjin hutu, %

-19

-16

-18

-21

-16

-15

Fuel C

Canjin girma/%

23 ℃/72h

Saukewa: ASTM D471

+22

+19

+18

+19

+19

+19

Yanayin Magani

Ƙara 0.7 sassa na bis (2+5), vulcanization mataki daya 170 ℃ × 15min, mataki biyu vulcanisation: 200 ℃ × 4h.

Ayyukan da aka ba da shawarar:


An ba da shawarar yin amfani da kashi 0.6 zuwa 1 na wakilin sinadarai na bisdipenta don vulcanization (2,5-dimethyl-2,5-bis(tert-butylperoxy)hexane).


Abokan ciniki yakamata su zaɓi mafi dacewa da zafin jiki da lokacin warkewa bisa girman samfurin da hanyar warkewa.


Kunshin samfur:


Wannan samfurin ba shi da haɗari, a maimakon haka ya ƙunshi kati, filastik, da kilogiram 10 a kowace jaka, jaka 2 a kowane akwati.


Shekarun ajiya:


Wannan samfurin yana da ƙarfin kwararar sanyi, ya kamata a guji jakar don kada ya lalace yayin sufuri ko amfani.


Ajiye a cikin sanyi, busasshiyar yanayi tare da tsawon rayuwar watanni 12.


Na baya: 
Na gaba: 

SAUKAR HANYA

KAYANMU

BAYANIN HULDA