FV9400
Herchy
| Disponibbiltà: | |
|---|---|
| Kwantità: | |
Oġġetti |
Indikaturi |
||||||
Gradi |
FV9430 |
FV9440 |
FV9450 |
FV9460 |
FV9470 |
FV9480 |
|
tad-Dehra |
Trasluċenti abjad ħalib |
Isfar |
|||||
Gravità speċifika / g / ċm3 |
ASTM D792 |
1.38 |
1.41 |
1.42 |
1.43 |
1.45 |
1.47 |
Ebusija/shoreA |
ASTM D2240 |
28 |
40 |
48 |
60 |
70 |
80 |
Qawwa tat-tensjoni/MPa |
ASTM D412 |
10.2 |
9.5 |
9.5 |
10.2 |
9.9 |
8.1 |
It-titwil fil-waqfa /% |
ASTM D412 |
485 |
494 |
363 |
296 |
241 |
159 |
Qawwa tad-dmugħ/KN/m |
ASTM D624-B |
18 |
26 |
19 |
22 |
21 |
16 |
Sett ta' Kompressjoni (177℃ * 22h) |
ASTM D395 |
9 |
8 |
8 |
7 |
8 |
9 |
Reżiljenza/% |
ASTM D1054 |
41 |
35 |
46 |
40 |
37 |
39 |
* Reżistenza għas-sħana |
Bidla fl-ebusija/xatt A |
+2 |
+2 |
+3 |
+2 |
+2 |
+3 |
Bidla fis-saħħa tat-tensjoni, % |
-18 |
-17 |
-21 |
-25 |
-20 |
-19 |
|
Titwil fil-bidla fil-waqfa, % |
-19 |
-16 |
-18 |
-21 |
-16 |
-15 |
|
Fjuwil Ċ Bidla fil-Volum/% 23℃/72h |
ASTM D471 |
+22 |
+19 |
+18 |
+19 |
+19 |
+19 |
Kundizzjoni tat-Tqaddid |
Żid 0.7 partijiet ta 'bis(2+5), vulkanizzazzjoni ta' stadju wieħed 170℃ × 15min, vulkanizzazzjoni f'żewġ stadji: 200℃ × 4h. |
||||||
Azzjonijiet rakkomandati:
Huwa ssuġġerit li tutilizza 0.6 sa 1 parti ta 'aġent kimiku bisdipenta għall-vulkanizzazzjoni (2,5-dimethyl-2,5-bis(tert-butylperoxy)hexane).
Il-klijenti għandhom jagħżlu l-aktar temperatura u ħin xierqa għall-ikkurar ibbażati fuq id-daqs tal-prodott u l-metodu ta 'tqaddid.
Ippakkjar tal-prodott:
Dan il-prodott mhuwiex perikoluż, huwa minflok magħmul minn kartun, plastik, u 10 kilogrammi għal kull borża, 2 boroż għal kull kaxxa.
Età tal-ħażna:
Dan il-prodott għandu kapaċità ta 'fluss kiesaħ, il-borża għandha tiġi evitata sabiex ma ssirx ħsara waqt it-trasport jew l-utilizzazzjoni.
Żomm f'ambjent frisk u niexef b'ħajja fuq l-ixkaffa ta' 12-il xahar.