FV9400
Herchy
| Beskikbaarheid: | |
|---|---|
| Hoeveelheid: | |
Items |
Aanwysers |
||||||
Grade |
FV9430 |
FV9440 |
FV9450 |
FV9460 |
FV9470 |
FV9480 |
|
Voorkomstoetsmetodes |
Melkwit deurskynend |
Geelagtig |
|||||
Spesifieke swaartekrag/ g/cm3 |
ASTM D792 |
1.38 |
1.41 |
1.42 |
1.43 |
1.45 |
1.47 |
Hardheid/kusA |
ASTM D2240 |
28 |
40 |
48 |
60 |
70 |
80 |
Treksterkte/MPa |
ASTM D412 |
10.2 |
9.5 |
9.5 |
10.2 |
9.9 |
8.1 |
Verlenging by breek /% |
ASTM D412 |
485 |
494 |
363 |
296 |
241 |
159 |
Skeursterkte/KN/m |
ASTM D624-B |
18 |
26 |
19 |
22 |
21 |
16 |
Kompressiestel (177 ℃ * 22 uur) |
ASTM D395 |
9 |
8 |
8 |
7 |
8 |
9 |
Veerkragtigheid/% |
ASTM D1054 |
41 |
35 |
46 |
40 |
37 |
39 |
* Hitteweerstand |
Hardheid verandering /shore A |
+2 |
+2 |
+3 |
+2 |
+2 |
+3 |
Treksterkte verandering, % |
-18 |
-17 |
-21 |
-25 |
-20 |
-19 |
|
Verlenging by breekverandering, % |
-19 |
-16 |
-18 |
-21 |
-16 |
-15 |
|
Brandstof C Volumeverandering/% 23 ℃/72 uur |
ASTM D471 |
+22 |
+19 |
+18 |
+19 |
+19 |
+19 |
Genesende toestand |
Voeg 0.7 dele bis(2+5) by, een-fase vulkanisering 170℃×15min, twee-fase vulkanisering: 200℃×4h. |
||||||
Aanbevole aksies:
Daar word voorgestel om 0,6 tot 1 deel bisdipenta chemiese middel vir vulkanisering (2,5-dimetiel-2,5-bis(tert-butielperoksie)heksaan) te gebruik.
Kliënte moet die mees geskikte temperatuur en tyd vir uitharding kies op grond van die produk se grootte en metode van uitharding.
Produk verpakking:
Hierdie produk is nie gevaarlik nie, dit bestaan eerder uit karton, plastiek en 10 kilogram per sak, 2 sakke per boks.
Ouderdom van berging:
Hierdie produk het 'n kouevloeivermoë, die sak moet vermy word om dit nie tydens vervoer of gebruik te beskadig nie.
Hou in 'n koel, droë omgewing met 'n raklewe van 12 maande.