Fluorosilicone Lastikuw FV9400

Nin fura in ye fluorosilicone elastomer ɲagaminen ye min bɛ kɛ basigi kola ye ani fasa ni faralifɛn suguya caman.
A fanga ka bon ani a bɛ se ka muɲu.
Tumu sɔrɔli ka ɲi kosɛbɛ, a bɛ se ka fɛnɲɛnamafagalanw kɛlɛ ani a bɛ se ka funteni caman ni funteni dɔgɔya.
  • FV9400 ye

  • Herchy (Herchy) ye

A sɔrɔli:
Hakɛ: .


Minɛns

Taamaʃyɛnw

Kalanso minnu bɛ sɔrɔ

FV9430 ye

FV9440 ye

FV9450 ye

FV9460 ye

FV9470 ye

FV9480 ye

Yecogo
sɛgɛsɛgɛli fɛɛrɛw

Nɔnɔ finman min bɛ yeelen bɔ

A bɛ kɛ jɛman ye

Gɛrɛsi kɛrɛnkɛrɛnnen/ g/cm3

ASTM D792 ye

1.38

1.41

1.42

1.43

1.45

1.47

Gɛlɛya/kɔgɔjidaA

ASTM D2240 ye

28

40

48

60

70

80

Tensile fanga/MPa

ASTM D412 ye

10.2

9.5

9.5

10.2

9.9

8.1

Elongation Ka Lafiɲɛbɔ /% .

ASTM D412 ye

485

494

363

296

241

159

Ɲɛjibɔ fanga/KN/m

ASTM D624-B ye baara kɛ

18

26

19

22

21

16

Set de compression(177°C * 22h) Bamako, Mali.

ASTM D395 ye

9

8

8

7

8

9

Ko ku/%

ASTM D1054 ye

41

35

46

40

37

39

*Fɛn sumaya kunbɛncogo ye
225°C×72h ye

Gɛlɛya caman yeli /shore A

+2

+2

+3

+2

+2

+3

Tensile fanga yeli, % .

-18

-17

-21

-25

-20

-19

Elongation at break changement, % 1000. Bamako, Mali.

-19

-16

-18

-21

-16

-15

Fuel C. Bamako

Volume Changement/% Bamako, Mali.

23°C/72h ye

ASTM D471 ye

+22

+19 ye

+18 ye

+19 ye

+19 ye

+19 ye

Kɛnɛyako cogoya

Aw bɛ bis(2+5) tilayɔrɔ 0,7 fara a kan, vulcanisation kɛcogo kelen 170°C×15min, vulcanisation kɛcogo fila: 200°C×4h.

Waleya minnu bɛ fɔ:


A jirala ko bisdipenta kemikɛlifɛn tilayɔrɔ 0,6 fo 1 bɛ kɛ ka vulkanize (2,5-dimethyl-2,5-bis(tert-butylperoxy)hexane) kɛ.


Kunnafonidila ka kan ka funteni ni waati min bɛnnen don kosɛbɛ furakɛli ma, o sugandi ka kɛɲɛ ni fura hakɛ ni a furakɛcogo ye.


Fɛn dilannenw foroko:


Nin fura in farati tɛ, a nɔ na, ​​a bɛ kɛ ni kariti ye, plastiki, ani kilo 10 bɔrɔ kelen kɔnɔ, bɔrɔ 2 kɛsu kelen kɔnɔ.


A marali san hakɛ:


Nin fura in bɛ se ka ji bɔ nɛnɛ na, bɔrɔ ka kan ka kɔlɔsi walasa a kana tiɲɛ a tacogo walima a baara waati.


Aw bɛ a mara yɔrɔ nɛnɛman ni jalen na, a marali waati bɛ se kalo 12 ma.


Tɛmɛnen: 
Nata: 

LINKS TELIKANW

AN KA FƐƐRƐW

KUNNAFONIW MINNU BƐ SƆRƆ

Fàra o kan: No.33, Lane 159, Taiye sira kan, Fengxian mara la, Shanghai
Telefɔni / WhatsApp / Skype: +86 15221953351
Hakilila-jɔ-sɛbɛn     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap (yɔrɔ karti). |   Kunnafoni dogolenw ka sariya | Dɛmɛn By Leadong ye.