FV9400
Herchy
| Dobavljivost: | |
|---|---|
| Količina: | |
Predmeti |
Indikatorji |
||||||
Ocene |
FV9430 |
FV9440 |
FV9450 |
FV9460 |
FV9470 |
FV9480 |
|
videza |
Mlečno bel prosojen |
Rumenkasto |
|||||
Specifična teža/g/cm3 |
ASTM D792 |
1.38 |
1.41 |
1.42 |
1.43 |
1.45 |
1.47 |
Trdota/ShoreA |
ASTM D2240 |
28 |
40 |
48 |
60 |
70 |
80 |
Natezna trdnost/MPa |
ASTM D412 |
10.2 |
9.5 |
9.5 |
10.2 |
9.9 |
8.1 |
Raztezek ob pretrganju /% |
ASTM D412 |
485 |
494 |
363 |
296 |
241 |
159 |
Trdna trdnost/KN/m |
ASTM D624-B |
18 |
26 |
19 |
22 |
21 |
16 |
Kompresijski set (177℃*22h) |
ASTM D395 |
9 |
8 |
8 |
7 |
8 |
9 |
Prožnost/% |
ASTM D1054 |
41 |
35 |
46 |
40 |
37 |
39 |
* Toplotna odpornost |
Sprememba trdote / Shore A |
+2 |
+2 |
+3 |
+2 |
+2 |
+3 |
Sprememba natezne trdnosti, % |
-18 |
-17 |
-21 |
-25 |
-20 |
-19 |
|
Sprememba raztezka pri pretrganju, % |
-19 |
-16 |
-18 |
-21 |
-16 |
-15 |
|
Gorivo C Sprememba prostornine/% 23 ℃/72 h |
ASTM D471 |
+22 |
+19 |
+18 |
+19 |
+19 |
+19 |
Stanje strjevanja |
Dodajte 0,7 delov bis(2+5), enostopenjska vulkanizacija 170℃×15min, dvostopenjska vulkanizacija: 200℃×4h. |
||||||
Priporočena dejanja:
Priporočljivo je uporabiti 0,6 do 1 del bisdipenta kemičnega sredstva za vulkanizacijo (2,5-dimetil-2,5-bis(tert-butilperoksi)heksan).
Stranke naj izberejo najprimernejšo temperaturo in čas sušenja glede na velikost izdelka in način sušenja.
Pakiranje izdelka:
Ta izdelek ni nevaren, namesto tega je sestavljen iz kartona, plastike in 10 kilogramov na vrečko, 2 vrečki na škatlo.
Starost shranjevanja:
Ta izdelek ima zmogljivost hladnega pretoka, zato se vrečke izogibajte, da se ne poškoduje med transportom ali uporabo.
Hranite v hladnem in suhem okolju z rokom uporabnosti 12 mesecev.