Hydrogenated nitrile rubber precompound kanye nenhlanganisela-HNBR
Irabha ye-nitrile ene-Hydrogenated (HNBR noma i-HSN) iwumkhiqizo we-hydrogenation kanye nokugcwaliswa kwebhondi ye-carbon-carbon double bond ochungechungeni lwamangqamuzana erabha ye-nitrile, ngakho-ke ibizwa nangokuthi irabha ye-nitrile egcwele kakhulu.
I-HNBR inokumelana kahle nowoyela (ukumelana kahle nowoyela kaphethiloli, izinto zokuthambisa, izinyibilikisi ezinuka kamnandi); futhi ngenxa yesakhiwo sayo esigcwele kakhulu, inokumelana nokushisa okuhle, ukumelana okuhle kakhulu kwamakhemikhali (ukumelana kahle ne-Freon, ama-acids nama-alkali), ukumelana okuhle kakhulu kwe-ozone, nokumelana okuphezulu nokuguqulwa unomphela ekucindezelweni; ngesikhathi esifanayo, i-HNBR nayo inamandla aphezulu, ukusebenza okuphezulu kokudabula. I-HNBR iphinde ibe namandla aphezulu, ukusebenza kwezinyembezi eziphakeme, ukumelana nokugqokwa okuhle kakhulu, njll. Ingenye yerabha esebenza kahle kakhulu iyonke.
I-Herchy Rubber inethimba lezobuchwepheshe elinolwazi olucebile ku-HNBR R&D. Singathuthukisa imikhiqizo yezinhlelo zokusebenza ezahlukene ngokwezidingo zamakhasimende. Futhi ujabulele idumela eliphezulu e-China nasemhlabeni.
| I-Herchy | Uhlobo lwe-Vulcanization | Okuqukethwe kwe-Acrylonitrile | I-Money viscosity | Ukuqina | Amandla aqinile | Ukwandisa ngesikhathi sekhefu | I-IRM 903 Ukushintsha ivolumu | Isethi yokucindezela | Isicelo | Umlingiswa |
| 150℃*72h | 150℃*72h ASTM D395 Uhlobo B | |||||||||
| Ibanga | % | I-ML(1+4)100℃ | Shore A | Mpa | % | % | % | |||
| I-HNBR-S6035 | Isibabule | 35 | 50~100 | 60 | 17-24 | 300-500 | <20 | <60 | Imikhiqizo embonini ye-oilfield, | Ubude obuhle, ukuzinamathela kahle, ukucutshungulwa okuhle kakhulu |
| I-HNBR-S7035 | Isibabule | 35 | 50~100 | 70 | 17-24 | 300-500 | <20 | <60 | Imikhiqizo embonini ye-oilfield, imboni yezimoto, ibhande |
Ukumelana nokukhathala okunamandla, Ukuzimela kahle, Ukucutshungulwa okuhle kakhulu |
| I-HNBR-S8035 | Isibabule | 35 | 50~100 | 80 | 17-24 | 300-500 | <20 | <60 | Ukubhoboza ipayipi izingqimba zokuzivikela, Ppressure accumulators |
Ukumelana nokucindezela okuphezulu, Ukuzinamathela okuhle |
| I-HNBR-S6043 | Isibabule | 43 | 50~100 | 60 | 17-24 | 300-500 | <10 | <60 | Uphethiloli wezimoto, Imikhiqizo embonini ye-oilfield |
Ukumelana nowoyela, Ukucubungula Okuhle kakhulu |
| I-HNBR-S7043 | Isibabule | 43 | 50~100 | 70 | 17-24 | 300-500 | <10 | <60 | Imikhiqizo embonini ye-oilfield, imboni yezimoto, |
Ukumelana nowoyela, Ukumelana nokukhathala okunamandla , Ukuzimela kahle |
| I-HNBR-S8043 | Isibabule | 43 | 50~100 | 80 | 17-24 | 300-500 | <10 | <60 | Ukubhoboza ipayipi izingqimba zokuzivikela, Ppressure accumulators |
Ukumelana nowoyela, Ukumelana nomfutho ophezulu, Ukuzinamathela kahle |
| I-HNBR-P6035 | I-Peroxide | 35 | 50~100 | 60 | 17-24 | 200 ~ 350 | <20 | <30 | Imboni yezimoto, imboni yokukhiqiza Izindiza |
Ukumelana nezinga lokushisa eliphezulu, ukucutshungulwa okuhle kakhulu |
| I-HNBR-P7035 | I-Peroxide | 35 | 50~100 | 70 | 17-24 | 200 ~ 350 | <20 | <30 | Imboni yezokwakha, ama-gaskets enjini, ama-O-rings, ama-Seals |
Ukumelana nezinga lokushisa eliphezulu, isethi enhle yokucindezela |
| I-HNBR-P8035 | I-Peroxide | 35 | 50~100 | 80 | 17-24 | 200 ~ 350 | <20 | <30 | Amapayipi okumba, ama-Pressure accumulators, |
Ukumelana nengcindezi ephezulu, ukumelana nezinga lokushisa eliphezulu |
| I-HNBR-P6043 | I-Peroxide | 43 | 50~100 | 60 | 17-24 | 200 ~ 350 | <10 | <30 | Uphethiloli wezimoto kanye nezinhlelo zokugcoba | Ukumelana nowoyela, Ukucutshungulwa Okuncomekayo, Isethi yokucindezelwa okuhle |
| I-HNBR-P7043 | I-Peroxide | 43 | 50~100 | 70 | 17-24 | 200 ~ 350 | <10 | <30 | Amagasket enjini, O-rings, Seals, Belt |
Ukumelana nowoyela, Isethi yokucindezelwa okuhle, Ukucutshungulwa okuhle kakhulu |
| I-HNBR-P8043 | I-Peroxide | 43 | 50~100 | 80 | 17-24 | 200 ~ 350 | <10 | <30 | Amapayipi okubhoboza, ama-Pressure accumulators |
Ukumelana nowoyela, Ukumelana nengcindezi ephezulu, ukumelana nezinga lokushisa eliphezulu |
1. Ibhande elingunxantathu
2. Vibration Isolators
3.
Izimpawu
4. Ipayipi elikwazi ukumelana nokushisa
5.
Ibhokisi lokuvikela ukumba
6. Amaphistoni amaphampu odaka
7.
Ukuvala ama-gaskets embonini yezimoto
8. Izigxivizo zeziteshi zikagesi
9.
Amapayipi e-hydraulic
10. Izimpawu ze-hydraulic
11. Amashethi ekhebula eziteshini zikagesi
12. Ukuphrinta kanye namarola endwangu
13. Izimpawu ze-aerospace
14. Izembozo
15.Fuel bladders