FV9502
I-Herchy
| Ukutholakala: | |
|---|---|
| Ubuningi: | |
Izinto |
Inkomba |
||
Inombolo yomkhiqizo |
FV9552 |
FV9562 |
|
Ukubukeka Izindlela Zokuhlola |
okuphuzi |
||
I-Gravity ethize/g/cm3 |
I-ASTM D792 |
1.42 |
1.43 |
Ukuqina/uguA |
I-ASTM D2240 |
52 |
61 |
Amandla Okuqina/MPa |
I-ASTM D412 |
10.2 |
9.4 |
Ukwelula Ngekhefu /% |
I-ASTM D412 |
330 |
280 |
Amandla Ezinyembezi/KN/m |
I-ASTM D624-B |
20 |
19 |
I-Compression Set (177℃*22h) |
I-ASTM D395 |
7 |
8 |
Ukuqina/% |
I-ASTM D1054 |
35 |
34 |
*I-Heat Resistance |
Ukushintsha kokuqina/ugu A |
2 |
2 |
Ukushintsha kokuqina/ugu A |
-24 |
-23 |
|
Ukwelula ngesikhathi sokushintsha kwekhefu, % |
-21 |
-20 |
|
I-Fuel C |
I-ASTM D471 |
22 |
21 |
Isimo Sokwelapha |
Izingxenye ezingu-0.5 ze-bis-2-5, i-vulcanisation eyodwa yesiteji 170℃×15min, i-vulcanisation yesiteji ezimbili: 200℃×4h |
||
Izenzo ezinconyiwe:
Kuphakanyiswa ukuthi kusetshenziswe izingxenye ezingu-0.4-0.7 ze-bisdisulfide (2,5-dimethyl-2,5-bis(tert-butylperoxy)hexane).
Amakhasimende kufanele akhethe izinga lokushisa elifanele kakhulu nesikhathi sokwelapha ngokusekelwe kusayizi womkhiqizo kanye nendlela yokwelapha.
Ukupakishwa komkhiqizo:
Lo mkhiqizo awuyona ingozi, kunalokho wakhiwe nge-cardstock, ipulasitiki, namakhilogremu angu-10 esikhwameni ngasinye, izikhwama ezingu-2 ibhokisi ngalinye.
Iminyaka yokugcina:
Lo mkhiqizo unamandla okugeleza okubandayo, isikhwama kufanele sigwenywe ukuze singalimazi ngesikhathi sokuthutha noma ukusetshenziswa.
Gcina endaweni epholile, eyomile eneshalofu impilo yezinyanga eziyi-12.