FV9400
Herchi
| Mavjudligi: | |
|---|---|
| Miqdori: | |
Elementlar |
Ko'rsatkichlar |
||||||
Baholar |
FV9430 |
FV9440 |
FV9450 |
FV9460 |
FV9470 |
FV9480 |
|
Tashqi ko'rinishni |
Sutli oq shaffof |
Sarg'ish |
|||||
O'ziga xos tortishish / g / sm3 |
ASTM D792 |
1.38 |
1.41 |
1.42 |
1.43 |
1.45 |
1.47 |
Qattiqlik / qirg'oqA |
ASTM D2240 |
28 |
40 |
48 |
60 |
70 |
80 |
Kuchlanish kuchi/MPa |
ASTM D412 |
10.2 |
9.5 |
9.5 |
10.2 |
9.9 |
8.1 |
Uzilishdagi cho'zilish /% |
ASTM D412 |
485 |
494 |
363 |
296 |
241 |
159 |
Yirtilish kuchi/KN/m |
ASTM D624-B |
18 |
26 |
19 |
22 |
21 |
16 |
Siqish to'plami (177 ℃ * 22 soat) |
ASTM D395 |
9 |
8 |
8 |
7 |
8 |
9 |
Chidamlilik/% |
ASTM D1054 |
41 |
35 |
46 |
40 |
37 |
39 |
* Issiqlikka qarshilik |
Qattiqlikning o'zgarishi / qirg'oq A |
+2 |
+2 |
+3 |
+2 |
+2 |
+3 |
Kuchlanish kuchi o'zgarishi, % |
-18 |
-17 |
-21 |
-25 |
-20 |
-19 |
|
Uzilishdagi cho'zilish o'zgarishi, % |
-19 |
-16 |
-18 |
-21 |
-16 |
-15 |
|
Yoqilg'i C Ovoz balandligi/% 23℃/72 soat |
ASTM D471 |
+22 |
+19 |
+18 |
+19 |
+19 |
+19 |
Qattiqlashuv holati |
0,7 qism bis (2 + 5), bir bosqichli vulkanizatsiya 170 ℃ × 15 min, ikki bosqichli vulkanizatsiya: 200 ℃ × 4 soat qo'shing. |
||||||
Tavsiya etilgan harakatlar:
Vulkanizatsiya uchun bisdipenta kimyoviy agentining 0,6 dan 1 qismigacha (2,5-dimetil-2,5-bis (tert-butilperoksi) geksan) foydalanish tavsiya etiladi.
Iste'molchilar mahsulotning o'lchami va quritish usulidan kelib chiqib, eng mos harorat va quritish vaqtini tanlashlari kerak.
Mahsulot qadoqlash:
Ushbu mahsulot xavfli emas, uning o'rniga karton, plastmassa va har bir sumka uchun 10 kilogramm, har bir qutiga 2 ta qopdan iborat.
Saqlash muddati:
Ushbu mahsulot sovuq oqim qobiliyatiga ega, tashish yoki foydalanish paytida uni shikastlamaslik uchun sumkadan qochish kerak.
Salqin, quruq muhitda saqlash muddati 12 oy.