GA-9331
Herchy
| Availability: | |
|---|---|
| Quantity: | |
Test: 1% of curing agent (50% paste of DBPMH in silicone gum), 175° x5minx15MPa
| Product parameters | |||||
| Product | GA-9331 | GA-9341 | GA-9351 | GA-9361 | GA-9371 |
| Appearance | MilkyWhite | ||||
| Williamplasticity | 120 | 150 | 180 | 210 | 240 |
| Hardness (ShoreA) | 30 | 40 | 50 | 60 | 70 |
| Density(g/cm3) | 1.12 | 1.14 | 1.17 | 1.20 | 1.21 |
| Tensile strength (MPa) | 8.0 | 8.5 | 8.5 | 8.0 | 7.0 |
| Elongation(%) | 800 | 600 | 500 | 400 | 300 |
| Tear strength (kN/m) | 18 | 18 | 20 | 20 | 20 |