GA-9331 irratti kan argamu
Herchy jedhamuun beekama
| Argamuu: | |
|---|---|
| Baay’ina: . | |
Qormaata: %1 kan fayyisu (%50 paastaa DBPMH silikoonii gogaa keessatti), 175° x5minx15MPa
| Parameetaroota oomishaa | |||||
| Oomisha | GA-9331 irratti kan argamu |
GA-9341 irratti kan argamu | GA-9351 irratti kan argamu | GA-9361 irratti kan argamu | GA-9371 irratti kan hundaa’edha |
| Mul'ina | MilkiiAdii | ||||
| Wiliyaampilaastikii |
120 |
150 |
180 |
210 |
240 |
| Jabina (ShoreA) . |
30 |
40 |
50 |
60 |
70 |
| Dandeettii(g/cm3) . | 1.12 |
1.14 |
1.17 |
1.20 |
1.21 |
| Jabina harkisaa (MPa) . |
8.0 |
8.5 |
8.5 |
8.0 |
7.0 |
| Dheersuu(%) . | 800 |
600 |
500 |
400 |
300 |
| Jabina ciccituu (kN/m) . | 18 |
18 |
20 |
20 |
20 |