GA-9331
Herchy
| Wiwa: | |
|---|---|
| Opoiye: | |
Idanwo: 1% ti oluranlowo imularada (50% lẹẹ DBPMH ni gomu silikoni), 175° x5minx15MPa
| Ọja sile | |||||
| Ọja | GA-9331 |
GA-9341 | GA-9351 | GA-9361 | GA-9371 |
| Ifarahan | MilkyWhite | ||||
| Williamplasticity |
120 |
150 |
180 |
210 |
240 |
| Lile ( ShoreA) |
30 |
40 |
50 |
60 |
70 |
| Ìwúwo (g/cm3) | 1.12 |
1.14 |
1.17 |
1.20 |
1.21 |
| Agbara fifẹ (MPa) |
8.0 |
8.5 |
8.5 |
8.0 |
7.0 |
| Ilọsiwaju(%) | 800 |
600 |
500 |
400 |
300 |
| Agbara omije (kN/m) | 18 |
18 |
20 |
20 |
20 |