Sɔhwɛ: 1% a ɛyɛ aduru a wɔde sa yare (50% a wɔde DBPMH a wɔde ahyɛ silicone gum mu), 175° x5minx15MPa
| Nneɛma a wɔyɛ no parameters | |||||
| Adwadeɛ | GA-9331 na ɛwɔ hɔ |
GA-9341 na ɛwɔ hɔ | GA-9351 na ɛwɔ hɔ | GA-9361 na ɛwɔ hɔ | GA-9371 na ɛwɔ hɔ |
| Mmaeɛ | MilkyWhite a ɛyɛ fɛ | ||||
| Williamplasticity a wɔde yɛ nneɛma |
120 |
150 |
180 |
210 |
240 |
| Nneɛma a ɛyɛ den (ShoreA) . |
30 |
40 |
50 |
60 |
70 |
| Nsuo a ɛyɛ den(g/cm3) . | 1.12 |
1.14 |
1.17 |
1.20 |
1.21 |
| Ahoɔden a wɔde twe ade (MPa) . |
8.0 |
8.5 |
8.5 |
8.0 |
7.0 |
| Ntrɛwmu(%) . | 800 |
600 |
500 |
400 |
300 |
| Ahoɔden a ɛtetew mu (kN/m) . | 18 |
18 |
20 |
20 |
20 |