GA - 9 3 31
Herchy ya go swana le
| Go hwetšagala: | |
|---|---|
| Palo: . | |
Teko: 1% ya moemedi wa go fodiša (50% ya peista ya DBPMH ka gare ga mare a silicone), 175 ° x5minx15MPa
| Ditekanyetšo tša setšweletšwa | |||||
| Setšweletšwa | GA - 9 3 31 |
GA - 9 3 41 | GA - 9 3 51 | GA - 9 3 61 | GA - 9 3 71 |
| Ponagalo | MilkyWhite ya | ||||
| Williamplasticity ya go dira dilo |
120 |
150 |
180 |
210 |
240 |
| Thata (LebopoA) . |
30 |
40 |
50 |
60 |
70 |
| Kitlano (g / cm3) . | 1.12 |
1.14 |
1.17 |
1.20 |
1.21 |
| Matla a go goga (MPa) . |
8.0 |
8.5 |
8.5 |
8.0 |
7.0 |
| Go telefatšwa(%) . | 800 |
600 |
500 |
400 |
300 |
| Matla a go gagola (kN/m) . | 18 |
18 |
20 |
20 |
20 |